Too little binder leaves a weak hot face; too much makes the lining sinter too deep. Learn how binder level affects lining life.

B2O3BINDERS

The binder is a small part of a ramming mass by weight, but it has a big effect on how the lining sinters.

Too little binder

  • The hot face sinters slowly or thinly.
  • Grains erode and metal can penetrate.
  • The lining may wear quickly at the slag line.

Too much binder

  • Sintering goes deeper into the wall.
  • The loose back layer gets thinner, so cracks can run further.
  • The lining can become more prone to thermal-shock cracking.

Typical levels

Boric acid in silica ramming mass is commonly used at around one percent by weight, adjusted for furnace size, operating temperature and sintering practice. Boron oxide grades use their own recommended level. Always follow the figure given for the specific grade.

Mixing at site (non-premix)

  • Weigh the binder; do not measure by eye.
  • Mix thoroughly so it is evenly spread.
  • Mix only what you will ram that shift.

Why premix helps

In premix and boron oxide grades, the binder is blended at the plant to a fixed level, which removes one source of variation between relinings.